# Fiberglassing project:  Suggestions wanted

**URL:** <https://forums.speedlife.net/t/fiberglassing-project-suggestions-wanted/248127>\
**Category:** Shift518 Automotive\
**Created:** [November 5, 2009, 7:39am UTC](https://forums.speedlife.net/t/fiberglassing-project-suggestions-wanted/248127 "2009-11-05T07:39:56Z")\
**Posts on this page:** 1\
**Showing post:** 44

<div class="post-metadata">

**Author:** ![FMFGSX](https://avatars.discourse-cdn.com/v4/letter/f/f6c823/32.png) [@FMFGSX](https://forums.speedlife.net/u/FMFGSX)\
**Post date:** [December 3, 2009, 2:10pm UTC](https://forums.speedlife.net/t/fiberglassing-project-suggestions-wanted/248127/44 "2009-12-03T14:10:51Z")

</div>

> [@Benefit for my daughter April 14th.](https://forums.speedlife.net/t/benefit-for-my-daughter-april-14th/24487/70):
>
> Noticed one of the skirts has a small kink in it. So the bottom is not completely straight across. Actually about 1/2" or so. Can I heat up the fiberglass with a heat gun and bend the kink out?

You could try and heat it you, clamp some wood behind it as a flat surface, then throw it under a heat lamp for some hours to give it time to form and then let it cool down on it’s own.

---